Pro tip: started wet curing my slabs in Phoenix after a guy at the batch plant said dry air was eating my mix
I used to just cover them with plastic and call it good until an old finisher told me the 110 degree air here pulls moisture out faster than the plastic can hold it, so now I keep them wet for 7 days and my surface cracks dropped way down, anyone else in dry climates doing something different?