S
6

The day I learned I'd been grinding my tungsten backwards for 6 months

I was at a fab shop in Tulsa watching an old-timer set up his TIG rig and noticed his tungsten was pointed opposite mine. He laughed and said I was basically trying to weld with the dull end. Has anyone else had a basic setup habit that took way too long to fix?
3 comments

Log in to join the discussion

Log In
3 Comments
owens.cameron
3/32" tungsten every time for 316 stainless. Your old-timer was right about the grind but wrong about the dull end - a flat grind actually holds the arc better on thin material.
5
nancy_ross
nancy_ross19d ago
Gotta disagree on the flat grind, I've had better luck with a slight point on 316.
7
nathanj56
nathanj561d ago
Not sold on the flat grind for 316 myself...
1