Showerthought: I annealed every blade for 3 years straight without letting it cool slow enough
Found out from a guy at the hammer-in in Johnstown that I was pulling them out of the vermiculite after 2 hours. He said leave it overnight, minimum. Did a test on a small camp knife and the edge held way better chopping through a 2x4. So I was basically skipping the whole point. What do you all use to hold the heat, and how long do you actually wait?