Rant: I stopped normalizing every piece I forge and my work got cleaner
Honestly for the first 3 years at my shop in Akron I normalized every single piece no matter what it was. Then last spring a guy named Dale who's been at the anvil for 40 years watched me dunk a bottle opener and asked why I was wasting the heat. He said plain carbon under 1/4 inch does fine air cooling, and normalizing cold-worked steel is only worth it when you've actually stressed it. I tried it on a batch of 20 hooks and ran a file test on a few, and they held up fine. Now I only normalize when I've really hammered a piece or it's a blade going into a quench. Anyone else change up their heat treat routine after someone called out the extra steps?